We really need a picture Laura, But if you are into adhesives, then there are 5 minute epoxys. For instance Devcon says:working time 5mins, handling time 15 mins, full strength 1hour http://www.amazon.co.uk/s/?ie=UTF8&k...l_50tp2f6k0g_e
They need clean rough surfaces, surface to surface, not edge to edge.
An alternative for anything except aluminium and kept away from your normal work, is soft solder. It can be cut into small pallions and used with a liquid flux meant for it, and very little heat from a torch, using sweat soldering to keep it hidden. Dennis.
Sorry, George, crossed you.
Last edited by Dennis; 03-07-2012 at 09:03 PM.