    Progress report - It all worked, and so much smoother than I first thought it would be.

    I still need to work on how to keep the pre-melted solder somewhat respectable instead of flowing everywhere, but I've got a couple of ideas for that.
    Also surprised that the stainless rod is such a bad heat conductor that I could hold it in place by hand (the other end of the rod) while soldering.

    Thank you all so much. This has been a real learning experience.
    Click image for larger version. 

Name:	PoolS1.jpg 
Views:	10 
Size:	45.5 KB 
ID:	13409

  2. #12
    Join Date
    Dec 2009
    Location
    Central London
    Posts
    8,845

    Default

    Thank you for you feed back. If needed, the stain on your pins due to heating can quickly be removed with a yellow radial disk on your hand held motor run slowly.

    https://www.google.com/search?client...+for+jewellers Dennis

  3. #13
    Join Date
    Mar 2011
    Location
    Manchester UK
    Posts
    937

    Default

    that looks great nice job

  4. #14
    Join Date
    Dec 2014
    Location
    South Australia
    Posts
    1,844

    Default

    They have come up well, good to see you managed to sort it out.

  5. #15
    Join Date
    Aug 2022
    Location
    India
    Posts
    7

    Default

    Thank you for this information, it was really good info.