Hello,
I recently went on a jewellery course and made a 2mm silver bangle, I have bought all the tools and I am trying to make a 3mm square wire bangle, however I cannon get the solder to flow, the joint is tight and clean, so I have put it down to either two things:
The flux - I have got borax powder and easy flo flux powder - How should i be using them / mixixng them?
or my torch - I have the standard torch from cooksons - is this good enough to heat this?
On a couple of occasions, the solder has balled up, other times it has done nothing!!
Many thanks in advance for your help! : )