Originally Posted by
WitchfordSilver
1. microweld
2. i don't use mine a lot so M.E.K just gets changed less than it should. even after 6 months in the booster it still seems to do it's job. same with the water, just top up as it's used. don't run large tips or two torches so does not seem to get through that much water.
3. only good for small jobs, great for jumps rings, a standard machine would not provide enough heat to melt scrap or casting, you need a much larger source of heat to do than. you get a high temp in a small flame so something bigger than a ring and i'd expect to have trouble getting it hot enough to solder.
4. Microweld (small things), cooks torch (medium and quick jobs), oxycon and propane with littletorch (larger bits and melting), big un-named torch for big things (not used at bench)