Pretreatment of a graphite crucible
Morning all.
I have a inherited an electric furnace for melting metals. I have had it safety tested and purchased some new graphite crucibles for its use. Question, do I pretreat the graphite crucible with borax powder in the same way as the ceramic scorifier?
Thanks so much,
Les.
Poor old Les
-
There's a lot of information here Les, If youncan separate the wheat from the chaff, so to speak. Dennis.
https://www.google.com/search?client...VjPC5EQ4dUDCAo
-
Thanks Dennis, the consensus appears to be 300 degrees in the oven for about an hour to drive out moisture then coated with borax.
Cheers.
Poor old Les