Hello all. I just made this ring today using permanent marker. I know there must be a more permanent solution. Any ideas? The metal is brass.
Sent from my BTV-W09 using Tapatalk
Hello all. I just made this ring today using permanent marker. I know there must be a more permanent solution. Any ideas? The metal is brass.
Sent from my BTV-W09 using Tapatalk
For brass, I'd look at tourmaline solution (or other antiquing solution) - mostly because I can't remember whether liver of sulphur would do the job.
Other options could include epoxy (or cold enamels) or oil-based printing ink - as used by a number of engravers.
Most of them will wear off over time though.
Just went to try a brass strip with Noirit, which is a sulphur containing agent. Didn't work. Dennis.
I've got some of this stuff that works on brass http://www.jpennyltd.co.uk/shopping/...tion.php?id=50
Deb
Thank you. Looks like this will work.
Sent from my FIG-LX1 using Tapatalk
Damn I just ordered some liver of sulfur. Oh well it wasn't expensive and the maker said there were some custom chemicals added so it still might work. Thanks.
Sent from my FIG-LX1 using Tapatalk