Hi pearlescene
Thanks for that tip on the book I will have a look at it and see if I can get a copy
I didn’t even know that polishing was a master craft by itself awesome
Thanks Mark
Type: Posts; User: globalmark; Keyword(s):
Hi pearlescene
Thanks for that tip on the book I will have a look at it and see if I can get a copy
I didn’t even know that polishing was a master craft by itself awesome
Thanks Mark
Hi pearlescene
Thanks for that tip on the book I will have a look at it and see if I can get a copy
I didn’t even know that polishing was a master craft by itself awesome
Thanks Mark
Hi Denis
Thanks so much for the reply I will have a look into those micro mesh sheets and the other
Compounds and go from there - I figured I didn’t have the correct compound or mops so I will...
Hi guys
I have successfully made my 2 wedding bands melted formed and soldered and finished with help here thanks -
I have made my bride a small 9k heart with the left over gold and polished the...
Hi Denis
Thanks for the reply
Ok I will try again - the joint is super clean and tight as used my cabinet makers trick pulling 800g sandpaper through joint so that is perfect - must be the...
Hi
Thanks for the reply
I thought I heated the whole ring first then around the joint and finally a quick blast onto the solder - I am in experienced in soldering and most I have done before was...
Hi guys
Hope someone can help I am making own wedding bands one 3-4mm wife 18k for her one 9k 7mm wise for me I have both solders but 1st time I soldered I melted side of ring I figured I got...
Thanks for that tip - thats awesome info much appriciated
regards `mark
Hi Dennis
Thanks for your reply - I have ordered a few tiny bits of small various hardness Of 9k and 18k from cooksons yesterday - Was so cheap for small amounts so ordered all types for future...
Hi guys
I have search everywhere inc google - like many I have done a bit with silver but want to make own wedding rings (basic bands) and know I need the correct 9k or 18k solder for the correct...