so if I have rolled it and made a mistake, what would you then do? fold over and roll again, or roll it into a ball and roll out?
Type: Posts; User: sparkleprints; Keyword(s):
so if I have rolled it and made a mistake, what would you then do? fold over and roll again, or roll it into a ball and roll out?
No, but it was a little while ago, so I am starting at the opposite end of the bangle, gradually heating side to side around to the area to be soldered, but as soon as I go near the solder it is...
its a silver bangle and I am using a blow torch like this...
Hi
Can anyone help, I am getting lots of air bubbles in my art clay some of which arent visible to the eye and only appear when i fire the item, often ruining it!
What am I doing wrong? if I...
Argh, please help as I am going slightly mad with frustration!
I am using silver soldeer strip and borax, heating the whole piece, ensuring it is clean, moving around to build the heat, the borax...
Hi
I have started a business selling my handmade jewellery and would really like to get sme jewellery gift boxes or bags with my logo printed on them.
Can anyone offer any advice of where to...
Hi
I am a bit short of cash but really want a tumbler, can this one be used for tumbling Art Clay Silver does anyone know?
ebay item 220729935407
I know Id need to buy shot etc.
Any...
Which silicone mould are you using?
Can you help me, I am thinking of experimenting with copper and was wondering, does it tarnish if worn next to the skin?
Does it need special treatment?
Hi
I am new to Art Clay and could do with some help!
I fired a piece of Silver Art Clay and afterwards it cracked through the middle, and eventually snapped in two when I was trying to polish...
Hi
I am new to Art Clay and could do with some help!
I fired a piece of Silver Art Clay and afterwards it cracked through the middle, and eventually snapped in two when I was trying to polish...