Porosity and really bad casts. Is it investment or something else.
Hi. Still struggling here.
Attached are photos of my issues
Attachment 13412Attachment 13413Attachment 13414
Attachment 13411
I'll try to be brief. Sterling silver metal. 50% new, 50% used.
3d print of Jamghe castable resin. Also tried Phrozen purple. Cured resin as per recommended. The print is perfect.
Plasticast invest. Following recommended everything. Deionized water. Temp 22-24 C. Followed times and degassing.
Burnout @ 730. Followed Plasticast recommended schedule. Have varied with longer holds and even higher temp.
Kayacast casting machine. Furnace melting. No borax as graphite crucible. Cast as quickly as I can.
But a lot of porosity on some, and less on others.
I'm at 700 M above sea level so suspected the vacuum.
Spoke to Kayacast as the machine doesn't get to 29 but we've eliminated that.
A new suggestion is the investment. I've had it for about 4-5 months. It has always produced light brown staining as shown.
No idea what causes that. It doesn't change, regardless of the burnout schedule.
So I'm at a loss about what to try next.
Any help would be extremely appreciated.