smelting report went lower than 18ct. need help please...
I was about to make a cuff with 18ct gold with a lot of scraps. I have asked to scrap dealers to test before the smelting. They confirmed they are mix of lower 18ct and higher 18ct.
Then I sent it to Assay office for Smelting service. and the result came out as 747.8 instead of 750.
:(|
I am seeking a replying to help below questions.
1. To get 18ct,
I presume I can melt this gold again with some pure gold. right?
By melting gold 3 times (smelting by Assay office, melting it with extra pure gold and lost wax casting), will the cuff soft and it might be a break? Will it affect the quality of the gold?
I presume the cuff has to be stronger than rings with a lot of movement.
2. If I go-ahead to add more pure gold, Can anyone please tell me how much pure gold I should add here?
3. Do you guys recommend to add a bit of pure gold when I work with a lot of known scraps to be safe for the future for the testing result?
Many many thanks to read this.
Gina