18 Apr 2015 - by Alex T.

casting

Excellent for casting.used same temps as for sterling silver.HOWEVER used normal cooling down times as per sterling silver and the whole tree was virtually destroyed with cracks etc. Googled before second tree.let it have a good cool down for about 35 -40 min, broke out with hammer,everything perfect.happy casting

49 out of 50 people found this review useful